Description | It is high build coal tar epoxy coating it gives excellent water resistance. |
Volume Solids | 65% |
DFT | 125 Microns |
Mixing Ratio | Base CA 3 : 1 |
Pot Life | 4-6 Hrs at 30°C and 65% relative humidity |
Spreading Rate | 5.2 Sq.m/ltr on a smooth surface |
Surface Dry | 4-5 Hrs at 30°C and 65% relative humidity |
Hard Dry | 24 Hrs at 30°C and 65% relative humidity |
Subsequent Coat | As per substrate condition recommended coating system |
RECOATING TIME - MIN | 24 Hrs at 30°C |
RECOATING TIME - MAX | 7 Days |
Fully Cured | 7 Days |
Shelf Life | Base: 12 months Hardner: 6 months |
Surface Preparation | Recommended primed surface should be free from oil, grease, salt and any other foreign matter. |
Applicable Industry | Maintanance |
Application Method | Brush/ Airless Spray |
Recommended Thinner | Harlepoxy Thinner |
Suggested Use | 1.  Recommended for application on underwater hull, even in conjunction with cathodic protection. 2.  Also can be used in the cargo holds blast tanks |